När du anställer en ansedd plasttillverkare, När du anställer en ansedd plasttillverkare. När du anställer en ansedd plasttillverkare, När du anställer en ansedd plasttillverkare, När du anställer en ansedd plasttillverkare. När du anställer en ansedd plasttillverkare, När du anställer en ansedd plasttillverkare. Här är några tips på hur du undviker defekter, för en nästan felfri produktionskörning.

Dessa tre faktorer avgör framgången eller misslyckandet för en produktionskörning:

  • Bearbetningen
  • Möglet
  • Materialet

Making sure each of these elements is functional before the molding process is key. This is why it’s important to partner with a plastics manufacturer you can trust. If you’ve worked with a disreputable or inexperienced manufacturer, you may have encountered these defects.

Common Processing-Related Defects:

Burn MarksImproper ventilation or extended heating of the mold can cause unsightly black or brown carbon deposits.

BlisteringToo much heat or inadequate cooling causes bubbles or raised imperfections.

StringingMuch like a hot glue gun, stringing happens when the nozzle is too hot and an excess strand of plastic attaches to the part.

Stress Cracking And CrazingExposure to high temperature for too long can cause the appearance of crackling or single cracks.

Cold SlugsWhen an extra tab of hot plastic becomes attached to the part, it causes a non-uniform area.

Sink Marks And VoidsPoor part design, non-uniform heating and/or inadequate cooling can cause depressions or hollows in a part.

Flow MarksWhen a part cools too quickly, it can cause a wavy pattern or discoloration in the part.

Common Mold Design And/Or Maintenance Defects:

FörhalningWhen the cooling system works improperly, the mold can cool unevenly, causing warped, bowed effect.

Drag MarksImproper or misaligned injector systems can cause scratches when the part is ejected from the mold.

JettingIncorrect gate size, length or placement can cause a snake-like line of plastic that cools at a different rate than the main part.

Short ShotAn injection blockage can cause the mold to be improperly filled, which creates an incomplete part, or a short shot.

Flash Or BurrsIf the mold is damaged, poorly designed or there is poor clamping force, a thin protrusion can form beyond the body of the part.

Defects Linked To The Materials:

Splay (Often CalledSilver Streaks”)These are circular marks caused by excess moisture in the resin. They appear where the molten plastic hits the mold cavity.

DelaminationThis is caused by moisture in the pellets. The result is a flaky, crumbly surface layer.

Color StreaksThis is just as the name suggests, random streaks of color in your part. This comes from poorly mixing resins and colorants, or non-uniform ingredients.

Contaminates Embedded In The MaterialThis is caused by flecks or particles foreign material that often originates in the barrel of the press.

DiscolorationThis is caused by residual color in the hopper, usually due to improper flushing or not flushing the hopper at all.

Förbi Kina mögel tillverkare

Om JasonMould Industrial Company Limited:

JasonMould är en av de bästa tillverkare av formsprutning av plast som erbjuder fantastiska tjänster till sina kunder när det gäller tillverkning av avancerade formverktyg. De exporterar sina verktyg till olika delar av världen och har blivit ett av de mest kända namnen i industrisektorn.

Förfrågan Kontakt:

Kontaktperson: James Yuan

Företagsnamn: JasonMould Industrial Company Limited

Adress: LongGang Village,LongXi Town,BoLuo County,HuiZhou City,GuangDong-provinsen, Kina

Telefon: 86-752-6682869

E-post: [email protected]

Hemsida: https://www.jasonmolding.com

Dela detta inlägg