사출 성형 부품의 흑색 반점 변색의 가능한 요인 분석

1. 기계

난방 제어 시스템이 통제 불능이기 때문에, 배럴이 과열되어 검은 색으로 분해됩니다.

나사 또는 배럴의 결함으로 인해, 용융된 물질이 고착되어 축적된다., 분해는 장시간 고정 가열로 인해 발생합니다.. Check whether the rubber head kit is worn or whether there are metal foreign matters in it

Some plastics, ABS와 같은, are cross-linked and coked by high heat in the barrel. They are difficult to melt under the condition of almost maintaining the original particle shape, and are crushed by screw and then entrained into the parts

2. 곰팡이

Mold exhaust is not smooth, easy to scorch, or the size of the gating system is too small, shear too much, resulting in coking

There are improper oil lubricants and release agents in the mold

3. 플라스틱

Too much volatile matter, too much humidity, too much impurity, too much recycled material, and polluted

4. 처리

If the pressure is too high, the speed is too high, the back pressure is too high and the speed is too fast, the material temperature will decompose.

The barrel should be cleaned regularly to remove additives that are less resistant than the plastic.

 

 

JasonMould Industrial Company Limited 정보

Jasonmould는 중국 금형 제작자 플라스틱 금형- 사출 금형, 다이 캐스팅 금형, 플라스틱 블로우 성형, 회전 성형, 의료 플라스틱 사출 성형, 투샷 플라스틱 사출 성형, 인서트 몰딩, 오버 몰딩, 금속 사출 성형, 마이크로 사출 성형, 분말 사출 성형, 세라믹 사출 성형, 액체 사출 성형, 허스키 사출 성형, 가정용 곰팡이, 주조 금형, 금형 도구 다이, 맞춤 금형, 중국 금형, 신속한 프로토 타이핑 도구, 플라스틱 프로토 타이핑 툴링, 펀치 프레스 툴링, 모바일 / 휴대폰 부품 용 다이 및 툴링, 자동차 부품, 진공 청소기, 충전식 도구, 전화기, 복사기, 컴퓨터, 멀티미디어 스피커, 및 기타 많은 전자 제품 및 가전 제품. 또한 플라스틱 제품 제조업체, 금형 제조업체 중국– 플라스틱 부품, 플라스틱 물 탱크, 플라스틱 공, 플라스틱 용기, 플라스틱 버클, 플라스틱 앵커, 플라스틱 걸이, 플라스틱 숟가락, 플라스틱 파이프 피팅, 플라스틱 텀블, 플라스틱 식기, 플라스틱 컵들, 플라스틱 병, 플라스틱 쟁반, 플라스틱 화장품 용기, 플라스틱 케이스, 플라스틱 식품 용기, 플라스틱 의자, 플라스틱 캡, 플라스틱 캡 폐쇄, 플라스틱 튜브, 플라스틱 수도관, 플라스틱 손잡이, 플라스틱 튜브, 플라스틱 유틸리티 박스, 플라스틱 선반 등.

접촉:
사람: 제임스 위안
회사: JasonMould 산업 회사 제한
더하다: 롱강 빌리지,LongXi 타운,BoLuo 카운티,혜주시,광동성, 중국
Tel: 86-752-6682869
이메일: [email protected]

대지: https://www.jasonmolding.com/custom-injection-molding/

이 게시물 공유